Home  |  About Us  |  Products  |  Services  |  FAQ’s  |  Gallery  |  Sitemap  |  Inquiry  |  Contact Us  
 
 
 
 Mortars For Acid Proof Brick /  Tile  /  Mandana Stone  
 Acid Proof Tiles  
 Acid Proof Bricks  
 Acid Proof Lining  
 Acid Proof Flooring  
 Acid Resistant Tiles  
 Acid Resistant Bricks  
 Acid Resistant Lining  
 Acid Resistant Flooring  
 Red Mandana Stone  
 Epoxy Lining  
 Epoxy Flooring  
 Epoxy Coating  
 Water Base Epoxy  
 Glass Flake Filled Lining  
 Glass Flake Lining  
 Glass Flake Coating  
 Grouts  
 Water Proofing  
 Liquid Applied Stainless Steel  316 Coating  
 P.U.Flooring  
 Water Base Polyurethane  
 Polyurethane Wall Coating  
 Polyurethane Flooring  
 Self Leveled Epoxy Flooring  Coating Linings  
 
 
 

 

 

 

  Mortars For Acid Proof Brick /  Tile /  Mandana Stone
 
 
CNSL MORTAR :-
°
INTRODUCTION:

This is a two -part chemical setting CNSL base mortar used for acid resisting brick lining, to protect most commonly used construction materials like RCC, MS, steel, brick masonry construction etc., from corrosive environment in modern chemical age. CNSL is resistant to acids, alkalis, and solvents, etc. at
temperature upto 170 C.

°
AREA OF APPLICATION:

CNSL is used for acid resistant brick/tile lining where maximum chemical resistance is required at most
economical cost. CNSL is most inexpensive among other resin base mortar, but at the same time is most suitable material also.

° PHYSICAL PROPERTIES:

 Color  Black
 Mix Ratio by wt. Sol to
 Powder
 1.3
 Compressive Strength kg/cm2  100Kg
 Flexural Strength kg/cm2  30
 Bond Strength kg/cm2  4
 Water Absorption  1%by wt.
 Max. Temp.  170 C
 Setting Time  18-24 Hrs.

°
METHOD OF APPICATION MIXING:

CNSL is prepared by mixing of solution & powder to form a workable mortar. Mixing ratio is 1 part solution to 3 parts powder by wt. This ratio can vary depending upon ambient temperature and working conditions. Use clean, dry mixing pan. Take required quantity of solution and add powder slowly and start mixing to get uniform paste like mortar. Do not mix large quantity, and then can be used within 20-30 minutes.

°
APPLICATION:

Ensure bricks or tiles are clean, dry and kept at the same temperature of CNSL. Apply mixed mortar on brick/tile in Even thickness on all sides for bedding & jointing with the same materials. Apply little more in
center so no air pockets are formed while its installation. For only joints filling, it is recommended to take great care that full depth is filled with the same. During & after completion of the application, the area must be kept dry and free from and other materials and traffic, which can affect setting & curing of CNSL.

°
CHEMICAL RESISTANCE:

CNSL will provide very good protection against most acids, alkali solvents, oil, fats, salts etc. However it is not recommended for protection against HF, fluoride salts etc.

° STORAGE & SHELF LIFE:

Always keep solution & powder in cool, dry place, away from direct sunlight and moisture. If stored in sealed container and bags, shelf life of solution will be 12 months, and shelf life of powder will be 4-5 months.

° PACKING Solution:

25 kgs and 200 kgs (NET) in good quality MS drums. Powder: 37.5 kgs (NET) in LDPE+HDPE bags.

°
HEALTH & SAFETY:

it is advisable to wear protective wears at the time of use of CNSL and all other our products. In case of contact with skin and eyes, wash with plenty of water and consult a doctor. This information, given above in good faith, is based on results gained from experience and tests. However, all recommendations or suggestions are made without guarantee since the conditions of use are beyond our control.
 
CHEMIPROTECT ENGINEERS
Contact at Works :-
Plot No. 2114, Phase III, G.I.D.C. Estate, Vatva,
Ahmedabad-(India) - 382445.
Call Us :- Works +91-79-25891689
Fax :- +91-79-25830002
E-mail us :- info@acidproofindia.com

chemiprotect@dataone.in

chemiprotect@gmail.com